Oxidation
Casting 33# Zirconium Corundum Brick AZS33#-Y
Composed
of 10% of inclined zircon single crystal, 70% of inclined zircon-corundum
eutectic phase and 20% of glass phase, the brick has feaures of
little impurity, compact structure, high-termperature glass phase
exudation, free from glass liquid and resist high temperature. The
products are widely used in parts of glass melting like pool wall,
pool bottom, flame space and feeding channel.
  
Side
Wall Brick |
Arch
Brick |
Zirconium Corundum Brick 41#Y |
| Chemical
Compositon (%) |
| ●AL2O3 Allowance |
●ZrO2 ≥32.0 |
●SiO2 ≤16.0 |
●Fe2O3 ≤0.2 |
●TiO2 ≤0.15 |
●Na2O ≤1.5 |
| Weight
/ Cubic (g/cm3) |
| ●PT≥3.40 |
●QX≥3.40 |
●MS≥3.50 |
●WS≥3.60 |
●WS*≥3.55 |
|
| Physical
Features: |
| ●Refractoriness
(℃)≥1710 |
●0.2
megapa Refractoriness under load(℃)≥1700 |
●Porosity(%)≤2 |
| ●Volume
Density (g/cm3)≥3.70 |
●Temperature
of glass phase exudation (℃)>1400 |
|
|